LSR Silicone Overmold Glass  - LSR Silicone To Glass
LSR Silicone Overmold Glass  - LSR Silicone To Glass
LSR Silicone Overmold Glass

Product Specification:
Model No. : CL-26AB- 8
Minimum Order Quantity :   2 KGS
Lead Time:7-10 Days
Payment Terms:   T/T ,Paypal ,Western Union
Package:   1KG/Bottle
Tel: +0086-138 -2374 -7978
Fax: 0086-755-81478372
E-mail: export@klbsilicone.com

Silicone Primer CL-26AB-8 


LSR Silicone To Glass 


Product Details


CL-26AB-8, Silicone primer, is mainly to bond platinum curing agent-added HTV /LSR silicone with PA(Nylon), Metallics, Polyester, PET, Bakelite, Epoxy, FRP(Fibre glass) etc.

Si+glass2


       


Product Advantage


Good adhesion Strength 

No partial bonding failure 

No primer trace on finished silicone products

Si+Glass                                                          

                                                           Waterproof Function 

                                                                                                       4 Hours water- boiling Tests 

                                                                                                       Waterproof Function                                                                                                                                                                                                                                                                                                        


   Stable Quality 

     3 times repetitive standard tests 

     Making your silicone products 99% ok rates

   Stable Quality primer



Product Specifications


Appearance:Transparent or Pasty gel  

Ratio:A:B=1:1

Solvent:Component solvent          

Viscosity:<20mpa.s            

Specifical gravity  : 0.95 g/cm3

Shelf life:6 months without cover opened(25℃).



Processing


1,Coating the CL-26AB-8 on the edge of the glass. 

2,Direct the LSR silicone on the edge the glass in the injection moulding machine ,

apply 120~180℃ degrees for 1-3 minutes to vulcanize the silicone rubber .

3,Trim the rough edges and wash clean the glass covers 

4, Place the glass covers in the ovens , apply 180~220℃  for 1- 2 hours , a silicone glass cover is done made . 




Attention


1, Please cap its cover immediately after use to avoid volatilization.          

2, Store the used and unused adhesive in separate way to lengthen the shelf life.                           

3, After the primer coated on the substrates, leave it volatilize completely before entering the mold, otherwise, there will be bubbles in the finished products 

4, Wash clean the substrates to remove dirts or oil to avoid bad adhesion.                                           



OUR ADVANTAGEService

Sorry,Here is the product description, there is no data!